Alloy information - Properties of Paliney 5

Properties of Paliney 5 Annealed Stress-Relieved Heat-Treated**
Density, nominal      
grams/cc 10.5 10.5 10.5
Dwt/cu. inches 111 111 111
Solidus Temperature,nominal      
Degrees Celsius 934 934 934
Coeff.of Linear Expansion      
/Degrees Farenheit (70-900),nom. 9.6x10(-6) 9.6x10(-6) 9.6x10(-6)
/Degrees Celcius (20-500),nom. 17.2x10(-6) 17.2x10(-6) 17.2x10(-6)
Modulus of Elasticity psi,nom. 16.5x10(6) 16.5x10(6) 16.5x10(6)
.1% Yield Strength,ksi 70-90 125-175 140-185
Ultimate Tensile Strength,ksi      
Wire .003-.020 dia. 100-120 135-185 150-195
Strip .003-.015 thick 100-120 135-185 150-195
Elongation,% in 2 inches      
Wire .003-.060 dia. 10 min. 1-5 1-5
Strip .003-.015 thick 10 min. 3 min. 2-10
Knoop Hardness, 100-gram load      
(50 grams under .005 thick)      
Wire .003-.060 dia. 160-230 240-330 275-335
Strip .003-.015 thick 160-230 240-330 275-335
Vickers Hardness, 100-gram load      
(50 grams under .005 thick)      
Wire .003-.060 dia. 160-220 230-320 265-320
Strip .003-.015 dia. 160-220 230-320 265-320

**From the Annealed or Stress-Relieved condition; Heat-treated conditions:750-800F for 45 to 90 minutes