Properties of Paliney 9 Stress-Relieved
Resistivity, normal, ohm-cmf 220
Microhm cm 36.6
Density, grams/cc, nominal 11.9
Dwt./cu. in., nominal 125
Solidus Temperature  
F, nominal 1950
C, nominal 1065
Coeff.of Lenear Expansion/  
Modulus of Elasticity, psi, nominal 17x10(6)
Proportional Limit, psi, nominal 120,000
Ultimate Tensile Strength, psi  
Wire .005-.015 dia. 140,000-160,000*
Elongation, % in 2" 12%
Knoop Hardness (100-gram load) 375-340*